How To Use
1. Metallic Yarn
Ironing | 140 degree 15 sec |
Dry Heat | 180 degree 60 sec |
Hot Water (Drying) | 90 degree 30 min |
Hand Washing | 0.5 % soap |
0.2 % sodium carbonate Anhydride (60 degree 30 min) | |
Rubbing | 200 gr 100 times |
Dry Cleaning | Trichloroethylene, Perchloroethylene, Petroleum Benzine (25D 30 min) |
Steaming | 100 degree 40 min |
Boiling Water | 30 in 1 hr |
2. Hot Stamping Foil
3. Glitter Powder
4. Metallic Scrubber
- Do not store near fire
- Dry after use
- PET film may be detached at first time use, please wash it before use.